Raney Nickel Catalyst: Complete Technical Guide
Preparation, structure (50-100 m2/g BET), and spray-coating on woven nickel mesh for alkaline electrolysis HER catalysis. Covers Ni-Al alloy casting, caustic leaching activation, and electrode sintering protocols.
RAS Thermal Co., Ltd.
Head of Applications
Raney nickel is a porous nickel catalyst with 50-100 m2/g BET surface area, made by leaching aluminum out of a Ni-Al alloy in NaOH. Every industrial alkaline water electrolyzer uses it as the hydrogen evolution reaction (HER) catalyst. Its dominance is structural, and easy to explain. No other cost-competitive material gives you high intrinsic HER activity in alkaline media, electrical continuity through the nickel skeleton, and compatibility with 25-30% KOH at 80-90 C all at the same time.
TL;DR: Raney nickel (Ra-Ni): 50-100 m2/g BET surface area, 1000x solid Ni. Produced by NaOH leaching of Ni-Al alloy. Spray-coated onto woven Ni201 mesh (30-60 mesh, 0.19-0.30 mm wire). Pyrophoric when dry, so store under water. Standard HER catalyst for AWE.
How Raney Nickel Is Made: Three Stages
1. Alloy Casting and Crushing. High-purity nickel (min 99.5%) and aluminum are induction-melted under argon at 1500 C and cast into ingots. A 50:50 wt% Ni-Al composition gives a mixture of NiAl3, Ni2Al3 and NiAl intermetallic phases. The NiAl3 phase content tracks directly with final catalyst surface area, which is why XRD verification is standard at this stage. For electrode coating applications, the ingot is then crushed and sieved to 20-100 um particle size.
2. Caustic Leaching (Activation). The crushed Ni-Al powder goes slowly into 20-25% NaOH at 50-80 C with continuous stirring. The reaction 2Al + 2NaOH + 2H2O to 2NaAlO2 + 3H2 selectively dissolves the aluminum and liberates hydrogen gas as it does. Watch the temperature, because it is the one variable that ruins everything. Above 100 C the nickel skeleton sinters and the surface area drops irreversibly. Leaching runs 2-4 hours, until hydrogen evolution ceases. The slurry is then washed with deionized water to pH neutral to strip out residual sodium aluminate.
3. Storage and Handling. Freshly leached Raney nickel leaves the wash still wet, loaded with adsorbed hydrogen and holding 50-100 m2/g BET surface area. Let it dry in air and it ignites spontaneously. It is pyrophoric, full stop. That is why commercial material is supplied and stored under deionized water or isopropanol. In electrode manufacturing we keep it wet right up to the moment it is mixed into the catalyst ink slurry and coated onto the nickel mesh substrates. Sintering stabilizes it. After that, it is no longer pyrophoric.
Coating Raney Nickel onto Woven Nickel Mesh
The Raney nickel catalyst is only half the electrode. The other half is the conductive substrate that holds it, and for alkaline water electrolysis that substrate is woven nickel mesh. Catalyst sitting on a nickel mesh current collector is the industry-standard electrode architecture in this field.
Mesh substrate specification: woven nickel mesh, 30-60 mesh per inch, 0.19-0.30 mm wire diameter, plain weave, Ni201 grade, electropolished finish. The polishing removes edge burrs, and edge burrs are what cause coating defects and diaphragm puncture. At this mesh count the openings run about 0.12-0.66 mm, enough for catalyst slurry infiltration while still retaining the coating.
Catalyst ink formulation: Raney nickel powder (20-50 um particle size, wet) mixed with PTFE dispersion at 5-15 wt% dry basis in a water/isopropanol solvent blend. The PTFE binder does two jobs. It glues the catalyst mechanically to the mesh, and it opens hydrophobic channels for gas release. Typical catalyst loading is 10-30 mg/cm2 on the mesh substrate.
Coating and sintering protocol: Apply the ink by pneumatic spray coating to a uniform 50-200 um layer thickness. Dry at 80 C to drive off the solvents. Hot-press the coated electrode at 100-150 C under 5-10 MPa. Then sinter at 300-350 C for 1-2 hours under N2 or Ar atmosphere. Sintering does the final bonding to the nickel mesh surface, and it decomposes the PTFE surfactant. What comes out is a porous, mechanically stable electrode structure.
Bottom line: Raney nickel on woven Ni201 mesh (30-60 mesh, 0.19-0.30 mm wire, electropolished) is the electrode architecture with the longest track record in AWE stacks targeting 60,000+ hour lifetimes. The catalyst supplies surface area. The mesh supplies mechanical integrity and uniform current distribution. Get both specifications right.
Frequently Asked Questions (FAQ)
What is Raney nickel and why is it the standard HER catalyst?
Raney nickel is a porous nickel catalyst with 50-100 m²/g BET surface area, roughly 1000x solid nickel, made by leaching aluminum from a Ni-Al alloy in NaOH. Nothing else at comparable cost combines high HER activity in alkaline media, electrical continuity through the nickel skeleton, and compatibility with 25-30% KOH at 80-90°C.
What mesh substrate should Raney nickel be coated onto?
Woven nickel mesh, 30-60 mesh per inch, 0.19-0.30 mm wire, plain weave, Ni201 grade, electropolished so the edge burrs that cause coating defects and diaphragm puncture are gone. This mesh count gives openings spanning roughly 0.12-0.66 mm across the band, enough for catalyst slurry infiltration while still holding the coating.
How is Raney nickel handled safely?
Freshly leached Raney nickel is pyrophoric once it dries. It ignites spontaneously in air. So it is supplied and stored under deionized water or isopropanol, kept wet until it is mixed into the catalyst ink, and only becomes stable and non-pyrophoric after sintering onto the electrode.
Page last updated: 2026-08-14
Related articles
Electrolyzer Electrode Material Selection Guide
Technical comparison of nickel woven mesh, knitted mesh, nickel foam, and stainless steel electrodes for alkaline water electrolysis. Selection criteria for stack OEMs.
TechnicalNi200 vs Ni201: Which Nickel Grade for Your Electrolyzer?
The 0.13% carbon difference between Ni200 and Ni201 determines whether your electrode wire survives 10,000 hours or fails at 20,000. Selection guide with chemical composition, grain-boundary corrosion data, and application recommendations.
Need electrode mesh for your project?
Tell us your specification. Same-day technical quote with Mill Test Certificate sample.